Specifications for a transformer, valve or steel structure give the steel grade in the standard of the manufacturer's country. The same stainless steel appears as 12Kh18N10T (12Х18Н10Т), X6CrNiTi18-10, 1.4541, AISI 321 or 06Cr18Ni11Ti. Cross-reference tables help find a substitute, but the systems almost never match exactly: chemical limits, impact toughness requirements and the thicknesses for which properties are guaranteed all differ.
How each system builds a grade name
| System | Example | What is encoded |
|---|---|---|
| GOST | 12Х18Н10Т | 0.12% carbon, about 18% chromium (Х), 10% nickel (Н), titanium (Т) |
| EN, name | S235JR, X6CrNiTi18-10 | S for structural, 235 for minimum yield strength in MPa; X for high-alloy, 0.06% C, 18% Cr, 10% Ni, Ti |
| EN, number | 1.4541 | steel number under EN 10027-2; 1.4xxx are stainless steels |
| AISI / ASTM | 304, 316L, 1045 | series number; L for low carbon; in carbon steels the last digits give carbon in hundredths of a percent |
| GB (China) | Q235B, 06Cr18Ni11Ti | Q for yield strength, B for quality grade; in stainless grades the leading digits give carbon in hundredths (two digits) or thousandths (three digits) of a percent |
GOST alloying letters: Г manganese, С silicon, Х chromium, Н nickel, М molybdenum, Т titanium, Ф vanadium, Б niobium, Ю aluminum, Д copper. A letter with no number after it means up to 1.5% of that element.
The suffix of EN structural steels gives the Charpy test temperature for 27 J: JR at +20 °C, J0 at 0 °C, J2 at −20 °C. In the Chinese system quality grades B, C, D and E play the same role. GB/T 1591-2018 replaced Q345 with Q355, which is closer to the European S355.
Common equivalents
| GOST | EN | AISI / ASTM | GB |
|---|---|---|---|
| St3sp (Ст3сп) | S235JR (1.0038) | A36 | Q235B |
| 09G2S (09Г2С) | S355J2 (1.0577) | A572 Gr 50 | Q355D |
| 20 | C22 (1.0402) | 1020 | 20 |
| 45 | C45 (1.0503) | 1045 | 45 |
| 40Kh (40Х) | 41Cr4 (1.7035) | 5140 | 40Cr |
| ShKh15 (ШХ15) | 100Cr6 (1.3505) | 52100 | GCr15 |
| 12Kh13 (12Х13) | X12Cr13 (1.4006) | 410 | 12Cr13 |
| 08Kh18N10 (08Х18Н10) | X5CrNi18-10 (1.4301) | 304 | 06Cr19Ni10 |
| 12Kh18N10T (12Х18Н10Т) | X6CrNiTi18-10 (1.4541) | 321 | 06Cr18Ni11Ti |
| 03Kh17N14M3 (03Х17Н14М3) | X2CrNiMo17-12-2 (1.4404) | 316L | 022Cr17Ni12Mo2 |
St3sp and S235JR are close in strength, but GOST 380 mainly governs chemistry, while the mechanical properties of rolled products come from separate product standards. 09G2S carries more silicon than S355J2 and is used down to −40…−70 °C when tested accordingly, so for cold climates the impact certificate is checked separately.
What to check before substituting
- Compare chemical composition under both standards, especially carbon, alloying elements, sulfur and phosphorus.
- Match yield and tensile strength for your thickness: guaranteed values drop as thickness grows.
- Check the impact test temperature and the impact energy.
- For welded structures, compare carbon equivalent and preheat requirements.
- For stainless steel, note titanium stabilization (321) or low carbon (304L, 316L): resistance to intergranular corrosion after welding depends on it.
- For pressure equipment and nuclear plants, substitutions are approved under industry codes; a cross-reference table is not enough there.
Customs codes for rolled steel and steel products are covered in the article on HS and UKTZED codes; enclosure protection in the IP, IK and NEMA guide.
Further reading
Discuss your project
Tell us about your challenge. We will help you find the right direction and define your next step.